BOSTIK 1200

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

BOSTIK 1200

Main features

  • 25% Joint-Movement Capability
  • 570% Cured Elongation
  • 10-Minute Tooling Window

Product Description

Bostik 1200 Acetoxy Cure Silicone Sealant is a one-component moisture-curing silicone designed for perimeter and joint sealing on non-porous construction surfaces. It develops adhesion to glass, glazed ceramic tile, and aluminum and cures to a flexible elastomer with 570% elongation and +/-25% joint movement capability under the documented test conditions. A 10-minute tool/work time supports placement and tooling, while the cured service-temperature range extends from -45 to 150 deg C. Applications include sealing around windows and doors, metal frames, skylights, and selected dissimilar-material joints within the supported substrate scope.

Key features

  • 25% Joint Movement: Demonstrates +/-25% joint movement capability under the documented joint-movement test.
  • 570% Cured Elongation: Provides 570% elongation at break after the documented 14-day cure condition.
  • 10-Minute Tooling Window: A 10-minute tool/work time supports placement and finishing before skin formation.

Applications

Perimeter sealing around windows and doors; sealing metal frames, windows and skylights; selected dissimilar-material joints within the documented substrate scope.

Product Family

BOSTIK 1200

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Translucent
Physical Properties
Skin Time
25 minutes
Mechanical Properties
Elongation
Elongation is the process of lengthening something. It is a percentage that measures the initial, unstressed, length compared to the length of the material right before it breaks. It is commonly referred to as Ultimate Elongation or Tensile Elongation at break.
570 %

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Tool / work time10minTypical uncured property
Skin time25minTypical uncured property
Flow / sag / slump0.1inTT-S-001543A / ASTM C639
Technical properties

Final-state properties

Typical cured properties after 14 days at 77 deg F and 50% RH unless otherwise noted.

PropertyValueUnitMethod / condition
Hardness17Shore AASTM D2240
Modulus at 100%58psiASTM D412
Tensile strength at break290psiASTM D412
Elongation at break570%ASTM D412
Joint movement capability+/-25%TT-S-001543A / ASTM C719
Service temperature-45 to 150deg CCured service range