BONDERITE S-ST 6776-LO

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

BONDERITE S-ST 6776-LO

Main features

  • Vertical and Overhead Surface Cling
  • Ready-to-Use Spray or Manual Application
  • Epoxy and Polyurethane Paint Removal

Product Description

BONDERITE S-ST 6776 LO AERO is a one-part, low-odor thixotropic paint stripper for removing epoxy, polyurethane, and other catalyzed coatings from approved aerospace metal substrates. The viscous green liquid is supplied ready to use and is designed to cling to vertical and overhead surfaces during spray or manual application. It can be used on aluminum, mild steel, cast iron, and titanium, while high-strength steel and magnesium are excluded from the documented substrate scope. Its chemistry contains no methylene chloride, chlorinated solvents, phenols, chromates, ammonia, or amines, supporting a differentiated stripping option for controlled aerospace maintenance processes.

Key features

  • Vertical and Overhead Cling: The thixotropic liquid is designed to remain on vertical and overhead surfaces.
  • Ready-to-Use Application: Supplied for spray or manual use without required mixing or dilution.
  • Catalyzed-Coating Removal: Removes epoxy, polyurethane, and other catalyzed paint systems from listed aerospace metals.

Applications

Removal of epoxy, polyurethane, and catalyzed paint systems from approved aluminum, mild steel, cast iron, and titanium surfaces by spray or manual application.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Viscous green liquid
Product Type
Material category or functional product class.
Paint stripper
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
>15,000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceViscous green liquidAs supplied
Brookfield viscosityGreater than 15,000mPa s20 deg C; 6 rpm
pH2.5 to 3.0As supplied
Optimal storage temperature5 to 35deg CStorage condition