BONDERITE S-AD 50

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

BONDERITE S-AD 50

Main features

  • Hydrochloric-Acid Pickling Inhibition
  • Non-Foaming Liquid Bath Additive
  • 1 to 6 g/L Process Concentration

Product Description

BONDERITE S-AD 50 is a non-foaming liquid inhibitor for hydrochloric-acid pickling processes. It is used to reduce acid attack on ferrous materials during pickling, including pretreatment ahead of electroplating or phosphating, and it is also suitable for selected cold-pickling applications on aluminum. The brownish liquid is typically used at 1 to 6 g/L in immersion baths and can operate at temperatures up to 85 deg C. A typical density of about 1.06 g/cm3 and a 24-month shelf life support practical bath preparation and storage planning.

Key features

  • Hydrochloric-Acid Pickling Inhibition: Reduces acid attack on ferrous materials during hydrochloric-acid pickling.
  • Non-Foaming Liquid Format: Supplied as a liquid inhibitor with non-foaming behavior for pickling-bath use.
  • Controlled Bath Concentration: Recommended at 1 to 6 g/L for immersion processing.

Applications

Hydrochloric-acid pickling inhibition for ferrous materials, including pretreatment before electroplating or phosphating; selected cold-pickling use on aluminum.

Technical Specifications

General Properties
Appearance
Appearance at room temperature.
Brownish liquid
Density (g)
1.06 g/cm3
Thermal Properties
Operating Temperature
up to 85 °C

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
AppearanceBrownish liquidAs supplied
DensityAbout 1.06g/cm320 deg C; DIN 51757
pHAbout 2.320% solution; 20 deg C
Recommended immersion concentration1 to 6g/LHydrochloric-acid pickling bath
Shelf life24monthsRecommended storage 0 to 40 deg C