BONDERITE M-AD 315
Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other
Main features
- Controlled Silicofluoride Bath Adjustment
- Defined 1.46 kg Addition Rate
- Immersion or Spray Phosphating
Product Description
BONDERITE M-AD 315 is a liquid metal-pretreatment additive used to increase silicofluoride content in zinc-phosphating baths. The colorless acidic solution has a density of 1.07 g/cm^3 and is suited to immersion or spray phosphating operations. For a 0.1 g/L silicofluoride increase in 1,000 L of bath volume, the process guidance calls for 1.46 kg, equivalent to 1.36 L, of additive. The product provides a defined bath-adjustment route where free fluoride, free acid, and total acid rise with the addition.
Key features
- Silicofluoride Bath Adjustment: Increases silicofluoride content in zinc-phosphating baths.
- Defined Addition Rate: Use 1.46 kg per 1,000 L to raise silicofluoride by 0.1 g/L.
- Immersion or Spray Use: Supports both immersion and spray zinc-phosphating operations.
Applications
Silicofluoride adjustment in zinc-phosphating baths used for immersion or spray processing.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Colorless solution | - | As supplied |
| Chemical character | Acidic solution | - | As supplied |
| Density | 1.07 | g/cm^3 | As supplied |
| Storage temperature | -10 to 40 | deg C | Unopened original packaging |
| Shelf life | 36 | months | Unopened original packaging |