BONDERITE L-GP 6041 CR
Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses
Main features
- Extended Indoor Corrosion Protection
- Non-Tacky Protective Film
- Dip Spray or Hand Application
Product Description
BONDERITE L-GP 6041 CR is a solvent-based corrosion inhibitor for extended protection of ferrous and galvanized alloys. The clear dark-brown concentrate is normally used as received and deposits a non-tacky film. Under normal production practices, indoor protection is typically up to 6 to 12 months, without treating that range as a specification. Dipping, spraying, and hand application provide flexible ways to cover metal surfaces, while most alkaline cleaning systems can remove the deposited material. The grade is suited to heavy-duty corrosion-protection operations requiring a durable temporary film.
Key features
- Extended Indoor Protection: Typically up to 6 to 12 months under normal production practices.
- Non-Tacky Deposited Film: The clear dark-brown concentrate is normally applied as received.
- Flexible Metal Application: Dipping, spraying, and hand application are supported for ferrous and galvanized alloys.
Applications
Corrosion protection of ferrous and galvanized alloys by dipping, spraying, or hand application.