BONDERITE C-AK 212

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

BONDERITE C-AK 212

Main features

  • Silicate-Free Aluminum Cleaning
  • Low-Etch Oil and Oxide Removal
  • Spray or Immersion Processing

Product Description

BONDERITE C-AK 212 is a concentrated, silicate-free, mildly alkaline liquid cleaner for aluminum and aluminum alloys. It removes oils and light oxide films while maintaining low etching characteristics, and its wetting agents do not emulsify oils and rinse readily from the metal surface. The cleaner can be applied by pressure spray or immersion, with an operating temperature range of 38 to 85 deg C (100 to 185 deg F). Its combination of silicate-free chemistry, low etching, and flexible application methods suits aluminum cleaning before subsequent surface treatment.

Key features

  • Silicate-free mild alkalinity: Concentrated liquid cleaning for aluminum and aluminum alloys.
  • Low-etch soil removal: Removes oils and light oxide films while limiting etching.
  • Spray or immersion use: Operates from 38 to 85 deg C (100 to 185 deg F).

Applications

Applications include spray or immersion cleaning of aluminum and aluminum alloys before subsequent surface treatment.

Product Family

BONDERITE C-AK 212

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Operating Temperature
38 - 85 °C