AXAREL 4000

Harmonization Code : 3909.20.00.90 | Amino-resins, phenolic resins and polyurethanes, in primary forms : Melamine resins : Other

AXAREL 4000

Main features

  • MIL-PRF-680 Type IV Cleaning
  • 147 deg F High-Flash Solvency
  • Low-Residue Heavy-Soil Removal

Product Description

AXAREL 4000 Solvent Cleaner is an approved MIL-PRF-680 Type IV solvent degreaser for high-flash-point cleaning of heavy greases, mineral oils, lubricants, coolants, synthetic fluids, and particulate soils. Its 147 deg F (64 deg C) flash point combines with a specific gravity of 0.77 and low vapor pressure of 0.8 mmHg at 20 deg C. The solvent is applied at full concentration by brush, pad, cloth, or immersion and soak equipment, providing a focused option for aviation and defense maintenance cleaning where strong solvency, controlled evaporation, and low surface residue are important.

Key features

  • Type IV qualification: Approved to MIL-PRF-680 Type IV for controlled solvent-degreasing requirements.
  • High-flash-point solvency: A 147 deg F (64 deg C) flash point accompanies strong removal of oils, greases, and particulate soils.
  • Full-concentration processing: Applies by brush, pad, cloth, or immersion and soak cleaning equipment.

Applications

Applications include commercial and general aviation cleaning, military and defense cleaning, and manual solvent cleaning.

Product Family

AXAREL 4000

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Thermal Properties
Flash Point
The flashpoint of a solvent is the lowest possible temperature at which it can vaporize to form an ignitable vapor. Flashpoint is often confused with “autoignition temperature”, which is the temperature at which a solvent ignites without an ignition source.
64 °C
General Properties
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
0.77
Vapor Pressure
0.8 mmHg
Physical Properties
Viscosity
Viscosity is a measurement of a fluid’s resistance to flow. Viscosity is commonly measured in centiPoise (cP). One cP is defined as the viscosity of water and all other viscosities are derived from this base. MPa is another common unit with a 1:1 conversion to cP. A product like honey would have a much higher viscosity -around 10,000 cPs- compared to water. As a result, honey would flow much slower out of a tipped glass than water would. The viscosity of a material can be decreased with an increase in temperature in order to better suit an application
1.54 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied properties at stated temperatures; values are not intended as specifications.

PropertyValueUnitMethod / condition
OdorMild citrus-Typical
Flash point147 (64)deg F (deg C)Typical
Specific gravity0.77-25 deg C; typical
Distillation range374 to 407 (190 to 205)deg F (deg C)Typical
Viscosity1.54cps25 deg C; typical
Vapor pressure0.8mmHg20 deg C; typical
Kauri-butanol value30-Typical
Nonvolatile residue60ppmTypical