ARALDITE DY026
Harmonization Code : 38159000 | Unspecified reaction initiators, accelerators, and catalytic preparations
Main features
- 110 to 115 g/eq Epoxy Equivalent Weight
- Difunctional Epoxy Reactive Diluent
- Composite and Electrical Epoxy Formulations
Product Description
ARALDITE DY 026 is a clear, low-viscosity difunctional reactive diluent for epoxy resins used in composite and electrical formulations. It has an epoxy equivalent weight of 110 to 115 g/eq by ISO 3001, density of 1.08 g/cm^3 at 25 deg C, and viscosity of 11 to 15 mPa s at 25 deg C by ISO 12058-1. Flash point is at least 156 deg C by ISO 2719. The material is also used as an adhesion promoter and flexibilizer in epoxy formulations, including high-temperature epoxy adhesive formulations.
Key features
- 110 to 115 g/eq epoxy equivalent: Epoxy equivalent weight is 110 to 115 g/eq by ISO 3001.
- 11 to 15 mPa s viscosity: Low as-supplied viscosity is 11 to 15 mPa s at 25 deg C by ISO 12058-1.
- Reactive formulation function: The difunctional diluent is used as an adhesion promoter and flexibilizer in epoxy formulations.
Applications
Epoxy formulation in composites, electrical applications, electrical components, and high-temperature epoxy adhesive formulations.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Additional Information
As supplied
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Physical form | Liquid | As supplied | |
| Appearance | Clear liquid | As supplied | |
| Epoxy equivalent weight | 110 to 115 | g/eq | ISO 3001 |
| Density | 1.08 | g/cm^3 | ISO 1675; 25 deg C |
| Flash point | >= 156 | deg C | ISO 2719 |
| Viscosity | 11 to 15 | mPa s | ISO 12058-1; falling ball; 25 deg C |
| Shelf life | 2 | years | Storage at 2 to 40 deg C |