ARALDITE AV8504

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

ARALDITE AV8504

Main features

  • Panel-Pin Aerospace Bonding
  • 10-Minute Minimum System Cure at 100 deg C
  • Sag-Resistant Toughened Epoxy System

Product Description

ARALDITE AV 8504 is the resin component of the ARALDITE AV 8504 / HARDENER TDT 177-27 two-component syntactic epoxy adhesive system for aerospace panel-pin bonding. When paired with TDT 177-27, the black thixotropic system provides sag resistance, high bond strength, toughness, and a resilient bondline. Recommended minimum cure times for the complete system include 15 hours at 25 deg C, 30 minutes at 60 deg C, and 10 minutes at 100 deg C. The system is intended for aerospace and panel applications with room- or elevated-temperature cure.

Key features

  • Aerospace panel-pin bonding: The AV 8504 / TDT 177-27 system is used for aerospace panel and pin bonding applications.
  • Temperature-dependent minimum cure: Recommended minimum cure is 15 hours at 25 deg C, 30 minutes at 60 deg C, or 10 minutes at 100 deg C.
  • Sag-resistant toughened system: The thixotropic system combines sag resistance, high bond strength, toughness, and a resilient bondline.

Applications

Resin component in the AV 8504 / TDT 177-27 system for aerospace and panel-pin bonding.

Technical Specifications

General Properties
Color
The color
Translucent white paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.19