ALPHA CNP CVP520

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

CNP CVP520

Main features

  • Low-Temperature 155 to 190 deg C Reflow
  • Extended 8-Hour Stencil Life
  • Air or Nitrogen Reflow

Product Description

ALPHA CVP-520 Solder Paste is a low-melting-point, no-clean, lead-free solder paste for low-temperature surface-mount assembly. Available configurations include multiple Sn/Bi/Ag alloy options with Type 3, Type 4, or Type 5 powder. Low-temperature processing uses peak reflow profiles between 155 and 190 deg C, and stencil life is more than 8 hours at 23 deg C and 50% RH. The paste is compatible with clean-dry air or nitrogen reflow. In suitable assemblies with temperature-sensitive through-hole components, CVP-520 can eliminate an extra wave or selective soldering process step.

Key features

  • Configurable paste: Available alloy configurations are paired with Type 3, Type 4, or Type 5 powder options.
  • Extended stencil life: Stencil life is more than 8 hours at 23 deg C and 50% RH.
  • Low-temperature reflow: Peak reflow profiles between 155 and 190 deg C can be run in clean-dry air or nitrogen.

Applications

Low-temperature surface-mount soldering and reflow assembly.

Product Family

ALPHA CNP CVP520

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Chemical Properties
Melting Point
Below 140°C

Additional Information

Technical properties

As-supplied and process properties

CVP-520 is offered in multiple alloy and powder configurations; exact processing details depend on the selected configuration.

PropertyValueUnitMethod / condition
Alloy options42Sn/57.6Bi/0.4Ag; 42Sn/58Bi; 42Sn/57Bi/1.0Ag on requestAvailable configurations
Powder typesType 3, Type 4, Type 5Available configurations
Stencil lifeMore than 8hours23 deg C; 50% RH
Refrigerated shelf life6months0 to 10 deg C
Stencil working temperature19 to 29deg CPrinting on stencil
Print speed40 to 100mm/secStandard and fine-pitch stencil printing
Peak reflow temperature155 to 190deg CGeneral effective range; configuration dependent
Reflow atmosphereAir or N2Clean-dry air or nitrogen