ABLESTIK A359

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

ABLESTIK A359

Main features

  • Up To 200 deg C Intermittent Use
  • 3-Minute 175 deg C Cure
  • 17.2 N/mm^2 Steel Shear Strength

Product Description

LOCTITE ABLESTIK A 359 is a one-component gray heat-cure structural epoxy adhesive for heat exchanger coil bonding, electric motor assembly, and pump or compressor component bonding. Typical cured shear strength is 17.2 N/mm^2 on steel and on aluminum, and 13.8 N/mm^2 on stainless steel. Its typical operating-temperature range is -40 to 175 deg C, with intermittent exposure up to 200 deg C. The paste exhibits zero sag with a 380 mil bead. Recommended cure schedules include 40 minutes at 135 deg C or 3 minutes at 175 deg C.

Key features

  • High-temperature service range: Typical operating range is -40 to 175 deg C, with intermittent exposure up to 200 deg C.
  • Accelerated heat cure: Recommended cure options include 40 minutes at 135 deg C, 30 minutes at 150 deg C, 10 minutes at 165 deg C, or 3 minutes at 175 deg C.
  • Metal shear strength: Typical shear strength is 17.2 N/mm^2 on steel and aluminum, and 13.8 N/mm^2 on stainless steel.

Applications

Heat exchanger coil bonding, electric motor assembly, and pump or compressor component bonding.

Product Family

ABLESTIK A359

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

Other Properties
Storage Temperature
-20 °C to-30 °C
General Properties
Appearance
Appearance at room temperature.
Gray paste
Specific Gravity
Specific gravity (SG) is the ratio of the density of a substance to the density of a reference substance; equivalently, it is the ratio of the mass of a substance to the mass of a reference substance for the same given volume. For liquids, the reference substance is almost always water (1), while for gases, it is air (1.18) at room temperature. Specific gravity is unitless.
1.5

Additional Information

Technical properties

As supplied

PropertyValueUnitMethod / condition
AppearanceGray pasteAs supplied
Specific gravity1.5As supplied
Extrusion rate100secondsTime to extrude 20 g
Sag0380 mil bead
Technical properties

Cured adhesive

PropertyValueUnitMethod / condition
Typical operating temperature-40 to 175deg CApplication range
Intermittent temperatureUp to 200deg CIntermittent exposure
Shear strength17.2N/mm^2Steel
Shear strength17.2N/mm^2Aluminum
Shear strength13.8N/mm^2Stainless steel