3M 810

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

3M 810

Main features

  • Visually Unobtrusive on Most Paper
  • 53% Renewable-Content Backing
  • Pen, Pencil, and Marker Writable

Product Description

Scotch Magic Tape 810 is a matte cellulose-acetate office tape with synthetic acrylic adhesive for permanent paper mending, document repair, envelope sealing, and labeling. Typical total thickness is 0.0625 mm, and typical elongation at break is 25%. The tape looks frosty on the roll but becomes visually unobtrusive on most paper; its matte surface accepts pen, pencil, and marker. The backing contains 53% renewable content by weight. For home, school, and office use, the applied tape is photo-safe and does not dry out or yellow with age.

Key features

  • 0.0625 mm total thickness: The typical tape construction combines a matte cellulose-acetate backing with synthetic acrylic adhesive.
  • Renewable-content backing: Renewable material accounts for 53% of the backing by weight.
  • Writable matte surface: Pen, pencil, and marker can be used for labels while the applied tape remains visually unobtrusive on most paper.

Applications

Permanent paper mending; document and photo repair; envelope sealing; labeling; general home, school, and office assembly.

Product Family

3M 810

Loading pricing…

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
The color
Soft White

Additional Information

Technical properties

As-supplied / before-processing properties

Legacy TDS values are typical and not current specifications; current-page values are scoped to the tape only.

PropertyValueUnitMethod / condition
BackingMatte cellulose acetate-Legacy exact-product TDS
AdhesiveSynthetic acrylic-Legacy exact-product TDS
Total tape thickness0.0625mmTypical legacy TDS value
Renewable content in backing53% by weightCurrent product page; tape only
Technical properties

After-processing / final-state properties

Legacy TDS values are typical and not current specifications; qualitative behavior follows the current product page.

PropertyValueUnitMethod / condition
Elongation at break25%Typical legacy exact-product TDS value
Applied appearanceVisually unobtrusive-On most paper
Surface writeabilityPen, pencil, or marker-Applied matte surface
Aging behaviorDoes not dry out or yellow-Current product-page statement

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers